Microscopy and Damage Analysis

Testing Systems

Test system System data Application
Stereomicroscope LEICA WILD M10 with digital camera DP27 and digital imaging software OLYMPUS Magnification range: (8 – 80) x
Lighting: Ring light and gooseneck
Damage analysis of elastomer and plastics. Documentation, image comparison, determination of size parameters
Stereomicroscope Binolupe LEITZ WETZLAR Magnification range: (12,5 – 100) x Deposit thickness measurements soot dispersal according to Firestone
Melting point microscope (microscope hot plate 350 LEITZ WETZLAR) temperature readout in the ocular Magnification: 60 x
hot plate temperature: RT – 350 °C polarisation
Determination of melting point or range
Stereo zoom microscope SZX 12 with digital camera DP 27 and digital imaging softare OLYMPUS Magnification range: (3,5 – 90) x
Lighting: LED ring light and gooseneck
Damage analysis of elastomer and plastics. Documentation, image comparison, determination of size parameters